Microcrystalline waxes are derived from residium. These waxes have very minute crystals (micro-crystals) and are flexible. They have a greater affinity for oil, which is held tightly in the crystalline lattice and does not migrate to the surface.
Microcrystalline Waxes are produced in a variety of melt points, colors, and penetration values. They will add a sensorial benefit to a formulation while improving oil retention.
Functions:
Flexible
Oil Retention
Forms Available:
Slabs
Pastilles
Compatibility:
Microcrystalline Wax is compatible with many vegetable and mineral waxes and a variety of natural and synthetic ingredients.
上海临辰医药科技有限公司 代理销售药用蜡:药用巴西棕榈蜡,白蜂蜡,黄蜂蜡,小烛树蜡,微晶蜡,石蜡, STRAHL & PITSCH, INC. 巴西棕榈蜡Carnauba Wax SP-63。巴西棕榈蜡SP63XFP
巴西棕榈蜡曾用于制备耐胃酸的微球。[1]其它:***用皮革等工业。酸值取本品,精密称定,置250ml烧瓶中,加二甲苯100ml,加热至完全溶解,加乙醇50ml和溴麝香草酚蓝指示液,加热使澄清后,趁热用乙醇制氢氧化钾滴定液()滴至绿色,并将滴定结果用空白试验校正。酸值(中国药典2005年版二部附录ⅦH)应为2~7。皂化值编辑取样品,精密称定,置250ml烧瓶中,加异丙醇-甲苯(5:4)混合液50ml,精密加入,加热回流3小时,加酚酞指示液1ml,趁热用盐酸滴定液()滴定剩余的碱,至溶液红色刚好褪去,加热至沸,如溶液又出现红色,再滴定至红色刚好褪去,并将滴定结果用空白试验校正。皂化值(中国药典2005年版二部附录ⅦH)应为78~95。鉴别取本品约,加*5ml,加热溶解,作为供试品溶液(趁热点样)。另取薄荷醇、麝香草酚各约10mg及乙酸薄荷酯10μl,置20ml量瓶中,加甲苯稀释至刻度,作为对照品溶液。照薄层色谱法(中国药典2005年版二部附录VB)试验,吸取供试品溶液6μl,对照品溶液2μl,分别点于同一硅胶G薄层板上,以乙酸乙酯-*(2:98)为展开剂,展开后,取出,晾干。 广东销售巴西棕榈蜡美国史东毕斯公司, 白蜂蜡 White Beeswax, SP-422G,NF。
石油蜡在内的各种蜡经物理改性制成的一种含蜡含水的均匀流体,是由石蜡与几种不同种类、性能的乳化剂及适当的调节剂经乳化反应制成的固-油-水多相分散体系的稳定乳状液,一般根据用途选用所需石蜡及乳化剂的种类。中文名石蜡乳液外观灰白色均质半透明液体固含量30%;50%PH值7-9抗酸、抗碱、耐硬水、水溶性强、乳液稳定,任意比例水稀释不分层、不破乳、不结块、保质期长、固含量高、分散性好。石蜡乳液技术指标编辑1、外观:灰白色均质半透明液体;2、固含量:30%;50%3、PH值:7-94、稳定性:用特殊中性非离子乳化,避免以前用碱性皂化不稳定、易分层的缺点,密封放置阴凉处可以存放两年不分层、不破乳、不结块。[1]石蜡乳液应用领域编辑随着“绿色化学”新慨念的提出与实施,石蜡乳液的开发我利用越来越受到人们的关注。人们认识到以水代替有机溶液剂作为蜡制品的载体,可**减少对生态环境的危害,所以乳化蜡的开发和利用前景十分广阔。石蜡乳液皮革业石蜡乳液可与加脂剂复配在加脂剂中复配少量的石蜡乳液改善和提高加脂剂的效果,通过试验证明,向皮革加脂剂中复配1%~5%的蜡乳液,可提高加脂剂的填充性能,提高加脂剂在皮纤维中的渗透性能,增加皮革的防水性能。
Test | Method | Specification |
---|---|---|
Color | Current Microcrystalline Wax NF monograph | Passes Test |
Melting Point | Current Microcrystalline Wax NF monograph | NF= 54 - 102 °C / SP-18NF= 73.9 - 79.4 °C |
Consistency | Current Microcrystalline Wax NF monograph | NF= 3 - 100 / SP-18NF= 55- 75 |
Acidity | Current Microcrystalline Wax NF monograph | Passes Test |
Alkalinity | Current Microcrystalline Wax NF monograph | Passes Test |
Residue on Ignition | Current Microcrystalline Wax NF monograph | NMT 0.1% |
Residual Solvents | Current Microcrystalline Wax NF monograph | None Detected |
Organic Acids | Current Microcrystalline Wax NF monograph | Passes Test |
Fixed Oils, Fats, and Rosin | Current Microcrystalline Wax NF monograph | Passes Test |
原标题:巴西棕榈蜡在食品涂层中的作用巴西棕榈蜡是一种黄色固体,质硬而脆,不溶于水的植物蜡片。巴西蜡是由生长在巴西东北部的皮奥伊州、塞阿拉州的巴西棕榈树的叶子上提取出来的蜡片,具有***的特性,能够适用于任何行业。巴西棕榈蜡是少数除小烛树蜡外硬度**高的一种天然蜡片,质地坚硬,具有极高的光泽性,易于乳化。其独有的抛光性能使它在食品、医药、家具、皮革等方面得到普遍应用。而在食品行业一般用做食品添加剂。在糖衣巧克力、糖果、口香糖等领域的脱模上有着***的应用。在我国,食品添加剂使用中规定:巴西棕榈蜡的功能为被膜剂和抗结剂,具体限量用法为,巴西棕榈蜡用于新型的可食用涂层中,涂在食品表面起到保鲜的目的。可以保持食品的新鲜度、口感、气味、质感以及营养价值。美国史东毕斯公司STRAHL & PITSCH, INC. 巴西棕榈蜡 Carnauba Wax SP-63XFP。广东进口石蜡
美国史东毕斯公司, 固体石蜡 Paraffin Wax, SP-1275,NF.巴西棕榈蜡SP63XFP
巴西棕榈蜡。1.性状:棕色至浅黄色脆性蜡,具有树脂状断面,微有气味2.密度(g/mL25ºC):3.相对蒸汽密度(g/mL,空气=1):未确定4.熔点(ºC常压):83-915.沸点(ºC,常压):未确定6.沸点(ºC,):未确定7.折射率(n20/D):8.闪点(ºC,):未确定9.比旋光度(º):未确定10.自燃点或引燃温度(ºC):未确定11.蒸气压(kPa,25ºC):未确定12.饱和蒸气压(kPa,60ºC):未确定13.燃烧热(KJ/mol):未确定14.临界温度(ºC):未确定15.临界压力(KPa):未确定16.油水(辛醇/水)分配系数的对数值(25℃):未确定17.上限(%,V/V):未确定18.下限(%,V/V):未确定19.溶解性(mg/mL):不溶于水。溶于热乙醇、热**、热氯仿、四氯化碳、油类。巴西棕榈蜡SP63XFP